1、 Overview:
Xng-100 plastic torsion tester is used to measure the torque applied to various thermoplastic samples within a specified time at a set temperature, and calculate the apparent rigidity modulus by measuring the torsion angle. And the influence of specimen distortion beyond the elastic limit and material creep properties.
2、 Applicable standards:
GB/T15047—94
3、 Main technical parameters:
1. Dial accuracy: 0.5 °
2. Incremental weight of weight: 0.1N
3. Sample size: 63.50 × six point three five × 1-3
4. Volume of thermos bottle: ≥ 1000ml
5. Thermometer accuracy: 1 ℃
6. Timer accuracy: 0.1s